Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.26e+15 ohm-cm | 3.26e+15 ohm-cm | |
ACC QSil 550R QSI Quantum Silicones Silicone Potting Material QSil 550Ris a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairab.. |