Electrical Properties Metric English Comments
Volume Resistivity 3.20e+13 ohm-cm
3.20e+13 ohm-cm
Taiwan PU Corporation TPUCO Polyurethane Sealing Resin
PU sealing resin is a waterproof, insulated protective film made of quality PU resin. It is used in the prevention of humidity, germs, collision, corrosion, parts loosening, and rusting, and as ins..
Volume Resistivity 3.20e+13 ohm-cm
3.20e+13 ohm-cm
ASTM D257
Teknor Apex Flexalloy® 89501-83FR Polyvinyl Chloride, Elastomer
Notes: 105°C Insulation; RoHS Compliant Features: High Heat Resistance; Low Temperature Flexibility Uses Wet Rated Insulation Wire Types: NISPE-1; NISPE-2; SE; SEO; SEOW; SEW; SJE; SJEO; SJEOW; S..
Volume Resistivity 3.20e+13 ohm-cm
3.20e+13 ohm-cm
ASTM D257
Teknor Apex APEX® 80128-Y Polyvinyl Chloride, Flexible
Notes: 75°C Insulation; RoHS CompliantFeatures: Sunlight Resistant (720 hours) Uses: Cable Jacketing; InsulationAgency Ratings: UL QMTT2 .E73402; UL 1063; UL 1581; UL 62; UL 83Forms: Pellets Wire..
Volume Resistivity 3.20e+13 ohm-cm

@Temperature 75.0 °C
3.20e+13 ohm-cm

@Temperature 167 °F
Tra-Con Tra-Bond 2159 Heat Conductive Electrically Insulating Compound
TRA-BOND 2159 is a flexible, thermal conductive epoxy system. It is used for staking transistors, diodes, resistors, integrated circuits and other heat-sensitive components to printed circuit boards..
Volume Resistivity 3.20e+13 ohm-cm

@Temperature 75.0 °C
3.20e+13 ohm-cm

@Temperature 167 °F
Tra-Con Tra-Bond 2158 Heat Conductive Electrically Insulating Compound
TRA-BOND 2158 is a flexible, thermal conductive epoxy system. It is used for staking transistors, diodes, resistors, integrated circuits and other heat-sensitive components to printed circuit boards..