Polymer Property : Volume Resistivity = 3.16e+9 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 3.16e+9 ohm-cm
3.16e+9 ohm-cm
ASTM D257
Tipco Tipcolite® TMHS 291 Phenolic Compound, Khaki Cotton Fabric, in fluffy form, Soft Flow & High Impact Strength
Soft Flow Phenolic Compound, Reinforced with Khakhi Cotton Fabric, in fluffy formApplications: Defence ApplicationsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Ind..