Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.16e+10 ohm-cm | 3.16e+10 ohm-cm | ASTM D257 |
Tipco Tipcolite® TG 211 Phenolic Compound, Mineral & Wood Flour, Soft Flow & High Electrical Properties Soft Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.. |
|||
Volume Resistivity | 3.16e+10 ohm-cm | 3.16e+10 ohm-cm | ASTM D257 |
Tipco Tipcolite® THD 321 Phenolic Compound, Wood Flour & Cellulose, having Soft Flow & High Strength Soft Flow Phenolic Compound, Reinforced with Wood Flour & CelluloseApplications: Switchgear, HRC FusesProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industries Lt.. |
|||
Volume Resistivity | 3.16e+10 ohm-cm | 3.16e+10 ohm-cm | ASTM D257 |
Tipco Tipcolite® TMS 111 Phenolic Compound, Cellulose Pulp, in fluffy form, having Soft Flow & High Strength Soft Flow Phenolic Compound, Reinforced with Cellulose Pulp, in fluffy formApplications: Defence ApplicationsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Volume Resistivity | 3.16e+10 ohm-cm | 3.16e+10 ohm-cm | ASTM D257 |
Tipco Tipcolite® TX 312 Phenolic Compound, Wood Flour & Minerals having Soft Flow & Lower Density Soft Flow Phenolic Compound, Reinforced with Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MouldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
I.. |
|||
Volume Resistivity | 3.16e+10 - 3.16e+11 ohm-cm | 3.16e+10 - 3.16e+11 ohm-cm | IS 3396-1979 |
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec.. |