Polymer Property : Volume Resistivity = 3.10e+11 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 3.10e+11 ohm-cm
3.10e+11 ohm-cm
ASTM D257-99
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which ena..
Volume Resistivity 3.10e+11 ohm-cm
3.10e+11 ohm-cm
ASTM D257-99
Rogers Corporation Poron® 4701-30-20064 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Contains PET film reinforcement. Standard available  thickness 0.064"Features and Benefits of PORON Products: Excelle..
Volume Resistivity 3.10e+11 ohm-cm
3.10e+11 ohm-cm
ASTM D257-99
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Volume Resistivity 3.10e+11 ohm-cm
3.10e+11 ohm-cm
ASTM D257-99
Rogers Corporation Poron® 4701-30-25047 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Volume Resistivity 3.10e+11 ohm-cm
3.10e+11 ohm-cm
ASTM D257-99
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which enab..
Volume Resistivity 3.10e+11 ohm-cm

@Temperature 50.0 °C
3.10e+11 ohm-cm

@Temperature 122 °F
ASTM D257
Teknor Apex APEX® 07-U0296A-65 Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Volume Resistivity 3.10e+11 ohm-cm
3.10e+11 ohm-cm
ASTM D247
Plenco 3303 Phenolic, Granular, Injection Molded
Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b..
Volume Resistivity 3.10e+11 ohm-cm
3.10e+11 ohm-cm
ASTM D247
Plenco 4304 Phenolic, Nodular, Transfer Molded
PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component ..