Electrical Properties Metric English Comments
Volume Resistivity 3.04e+14 ohm-cm
3.04e+14 ohm-cm
C 96/23/96
Abatron AboCast 8103-14 One-Component Epoxy
AboCast 8103-14 is the lowest-viscosity one-component epoxy system with heavy-duty structural and dielectric properties. It is clear and has maximum wetting and penetration. Suggested Uses: Casting..