Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.90e+13 ohm-cm | 2.90e+13 ohm-cm | |
Fujipoly Industries Sarcon® 25G-Td Thin-Film GR-TD Sarcon 25G-Td is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |