Polymer Property : Volume Resistivity = 2.60e+9 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 2.60e+9 ohm-cm

@Temperature 50.0 °C
2.60e+9 ohm-cm

@Temperature 122 °F
ASTM D257
Teknor Apex APEX® 65015 Polyvinyl Chloride, Flexible
Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex