Polymer Property : Volume Resistivity = 2.40e+15 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 2.40e+15 ohm-cm
2.40e+15 ohm-cm
Tra-Con Tra-Bond 2125 Rigid Syntactic Repair Adhesive
TRA-BOND 2125 is a medium viscosity, low density syntactic foam epoxy formulation developed for industrial, electronic and aerospace honeycomb, fillet, edge-fill, contour repair, bonding and casting..