Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.13e+13 ohm-cm | 2.13e+13 ohm-cm | IEC 60093 |
Gromax 1155LL TPE 1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex.. |