Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.10e+13 ohm-cm | 2.10e+13 ohm-cm | Condition A; IPC 2.5.17.1 |
Rogers Corporation RT/duroid® 5880LZ Lightweight, High Frequency PTFE Laminate RT/duroid® 5880LZ filled PTFE composites are designed for exacting stripline and microstrip circuit applications. The unique filler results in a low density, lightweight material for high performa.. |
|||
Volume Resistivity | 2.10e+13 ohm-cm | 2.10e+13 ohm-cm | |
Dow Corning 730 SOLVENT RESISTANT SEALANT Fluorosilicone (solvent resistant) RTV sealantInformation provided by Dow Corning |