Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+6 ohm-cm
2.00e+6 ohm-cm
PVCH/QCD/3519
Reliance Industries 67-11 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications: Recommended:Flexible extrusionFlexible injectionFlexible calenderingCan be used:Rigid injectionRigid extrusion
Volume Resistivity 2.00e+6 ohm-cm
2.00e+6 ohm-cm
Shinil Chemical SHINCON PES-CNT LCD Rack
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b..
Volume Resistivity 2.00e+6 ohm-cm
2.00e+6 ohm-cm
PVCH/QCD/3519
Reliance Industries 70-21 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications:Can be used:Flexible extrusionFlexible injectionFlexible calendering