Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.00e+18 ohm-cm @Temperature 23.0 °C |
2.00e+18 ohm-cm @Temperature 73.4 °F |
DAM; IEC 60093 |
DuPont Performance Polymers Zytel® 70G35EF NC010 Nylon 66
(Unverified Data**) Zytel® 70G35EF NC010 is a 35% glass reinforced polyamide 66 developed for electrical and electronics applications.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | 2.00e+18 ohm-cm | 2.00e+18 ohm-cm | ASTM D257 |
Styron CALIBREâ„¢ 200-14 Polycarbonate Resin Overview: CALIBREâ„¢ 200-14 polycarbonate resin is a natural, FDA compliant, 14 melt flow rate general purpose polycarbonate resin with no mold release or UV stabilizer.Govt. and Industry Standar.. |