Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 12 ohm-cm | 12 ohm-cm | |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/03 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Volume Resistivity | 12 ohm-cm | 12 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY 63000CT PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications |