Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.98e+15 ohm-cm | 1.98e+15 ohm-cm | Condition A; IPC TM-650 2.5.17.1 |
Arlon 25N Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |