Polymer Property : Volume Resistivity = 1.60e+9 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.60e+9 ohm-cm
1.60e+9 ohm-cm
Master Bond UV15SP-1 Low Viscosity, UV Curable System
Description: Master Bond UV15SP-1 is a new one component, high strength UV curable epoxy resin based polymer system for bonding, sealing, & coating with high performance properties. It is a 100% rea..