Electrical Properties Metric English Comments
Volume Resistivity 1.60e+12 ohm-cm
1.60e+12 ohm-cm
ASTM D257
PolyOne Geon™ Vinyl Wire & Cable 1802-xx05FRD Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Volume Resistivity 1.60e+12 ohm-cm
1.60e+12 ohm-cm
ASTM D247
Plenco 00755 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755..