Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.5 ohm-cm | 1.5 ohm-cm | DIN IEC93 |
P & P Technology CB 70 Carbon Loaded Silicone Applications: Electrically conductive grades which when properly catalyzed can be considered for applications requiring conductivity such as EMI gaskets, conductive sheaths for ignition cable core,.. |
|||
Volume Resistivity | 1.5 ohm-cm | 1.5 ohm-cm | ASTM D257 |
LNP VALOX® SMV5847 PBT + PET Alloy, 30% Carbon Fiber Reinforcement
(discontinued **) ESD Applications. VC3000.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data .. |