Polymer Property : Volume Resistivity = 1.46e+13 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.46e+13 ohm-cm
1.46e+13 ohm-cm
Dow Corning 3099 HVIC COMPOUND
Dow Corning 3099 is a grease-like silicone coating especially formulated to give electrical insulators long-term resistance to water filming and flashover.Features: Protecting electrical insulators...