Electrical Properties Metric English Comments
Volume Resistivity 1.40e+16 ohm-cm
1.40e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics NORYL WCD795 PPE-TPE (Asia Pacific)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as cable jacket of UL 62 SVE and NISPE confiations. Flame retardant performance capable of m..
Volume Resistivity 1.40e+16 ohm-cm
1.40e+16 ohm-cm
IEC 60093
SABIC Innovative Plastics Ultem ATX202R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Volume Resistivity 1.40e+16 ohm-cm
1.40e+16 ohm-cm
IEC 60093
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Volume Resistivity 1.40e+16 ohm-cm
1.40e+16 ohm-cm
IEC 60093
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Volume Resistivity 1.40e+16 ohm-cm
1.40e+16 ohm-cm
Master Bond EP46HT Epoxy Adhesive for Structural Bonding
Description: Master Bond System EP46HT is a newly formulated two component high performance heat resistant epoxy resin system with excellent mechanical strength and chemically resistant properties f..