Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.0e+15 ohm-cm | 1.0e+15 ohm-cm | VDE 0303 |
GEHR Plastics PE-HD Polyethylene HDPE Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature is from -50.. |