Polymer Property : Volume Resistivity = 1.0e+11 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.0e+9 - 1.0e+11 ohm-cm
1.0e+9 - 1.0e+11 ohm-cm
IEC 60093
Quadrant EPP Semitron® ESd 225 POM-C, static dissipative, extruded (ISO Data)
Semitron ESd 225 is an acetal based static dissipative material ideal for material handling operations. It is also an excellent choice for fixturing used in the manufacturing of hard disk drives or ..
Volume Resistivity 3.2e+10 - 1.0e+11 ohm-cm
3.2e+10 - 1.0e+11 ohm-cm
IS 3396-1979
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App..