Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+20 ohm-cm | 1.00e+20 ohm-cm | ASTM D257 |
Manifattura Cattaneo PTFE Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Volume Resistivity | 1.00e+20 ohm-cm | 1.00e+20 ohm-cm | ASTM D991 |
LyondellBasell Petrothene® LR686001 High Density Polyethylene ApplicationsPETROTHENE LR686001 is designed for use as insulation for foam/skin telephone singles, and is a natural, expandable, high density polyethylene compound containing a chemical blowing agen.. |