Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.13 ohm-cm | 0.13 ohm-cm | Chomerics MAT-1002 |
Parker Chomerics CHOFORM® 5560 Conductive Form-in-Place Gasket Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |