Electrical Properties Metric English Comments
Volume Resistivity <= 0.080 ohm-cm
<= 0.080 ohm-cm
Parker Chomerics CHO-BOND 4660 Conductive Caulk/Sealant
CHO-BOND® 4660 caulking compound is a single-component, electrically conductive, paste-like material intended for EMI shielding and grounding applications. Its non-hardening characteristic makes it..
Volume Resistivity <= 0.080 ohm-cm
<= 0.080 ohm-cm
Parker Chomerics CHO-BOND 4669 Conductive Caulk/Sealant
Chomerics two-component conductive epoxy caulks provide excellent adhesion to dissimilar substrates and can be used in lap or butt joint applications. They feature large silver-plated-copper particl..