Electrical Properties Metric English Comments
Volume Resistivity <= 0.070 ohm-cm
<= 0.070 ohm-cm
Epoxy Technology EPO-TEK® N20E Electrically Conductive Paste
Product Description: EPO-TEK® N20E is a two component, electrically and thermally conductive, epoxy adhesive designed for semiconductor and electronics assembly. Its applications and field conditi..