Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.0109 ohm-cm | 0.0109 ohm-cm | Printed onto 125µm PET film using 18cm<sup>3</sup>m<sup>-2</sup> anilox |
Gwent Electronic Materials C2080529D7 Carbon Flexographic Ink Carbon conductor ink specifically designed for printing on to polymeric or paper substrates using flexographic printing. Ink can be printed at speeds up to 20m/min, with good line definition and go.. |