Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.000020 ohm-cm | 0.000020 ohm-cm | |
Gwent Electronic Materials C2011009D1 Curable Silver Range This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive adhesive that combines good adhesion with excellent electrical properties.. |