Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.000011 ohm-cm | 0.000011 ohm-cm | |
H.C. Starck HPM 1801 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Volume Resistivity | 0.000011 ohm-cm | 0.000011 ohm-cm | At 2.50% Silicon |
Dura-Bar G2 Continuously Cast Gray Iron Bar Stock ASTM A48 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as an alternative to gray i.. |