Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.00000560 ohm-cm | 0.00000560 ohm-cm | |
Misumi ANP79 Aluminum Alloy Similar in hardness to 7075 Aluminum Alloy with lower internal stresses. Higher uniformity than 7075.Information provided by MISUMI Corporation. |