Polymer Property : Dielectric Strength = 980 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 38.6 kV/mm
980 kV/in
3M Scotch-Weld™ 2158 B/A Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2158 B/A is a gray, two-part, high strength adhesive that chemically cures at room temperature. It has good adhesion to a variety of substrates including metals, ma..