Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 38.2 kV/mm @Thickness 1.60 mm |
970 kV/in @Thickness 0.0630 in |
ASTM D149 |
Solvay Specialty Polymers Xydar® MG-350 Liquid Crystal Polymer, Mineral and Glass Filled
(discontinued **)< XYDAR MG-350 Liquid Crystal Polymer (LCP) is a mineral and glass-filled injection molding grade developed specifically for cost-effective performance in applications where a balance of flatness and .. |