Polymer Property : Dielectric Strength = 925 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 36.4 kV/mm
925 kV/in
Full-wave Impulse; ASTM D3426
DuPont™ Nomex® E56 Paper, 7 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..