Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 34.5 kV/mm | 876 kV/in | IEC 60243-1 |
Lanxess Durethan® DP 1852/30 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glassfibers, UL V-0 at 0.75 mm (listed),GWIT:775°C at 0,75 mm, GWFI:960°C at 0.75 mm, CTI/A:400, good flowabilityApplication Examples: Hand-held barrel pump housings |