Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 34.3 kV/mm | 870 kV/in | ASTM D149 |
Arlon MT920-10#3.3-P1 0.020" (0.508 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Description:0.020” thick x 1.0” wide x 3.33 yards long, Rectangular cross-section, Silicone, Self-Fusing Tape.Design/Construction: Interleave: Polyethylene Rubber: Cured Self-Fusing Silicone Rubbe.. |
|||
Dielectric Strength | 34.3 kV/mm | 870 kV/in | ASTM D149 |
ExxonMobil Santoprene® 211-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Dielectric Strength | 34.3 kV/mm | 870 kV/in | ASTM D149 |
ExxonMobil Santoprene® 221-64W175 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed .. |