Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 34.0 kV/mm | 863 kV/in | ASTM D149 |
Arlon 44141R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent.. |