Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 33.7 kV/mm | 855 kV/in | ASTM D149 |
Arlon 51344R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Semi-Cured Silicone RubberSubstrate: Style 7628 FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values fo.. |