Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 33.4 kV/mm | 848 kV/in | ASTM D149 |
Arlon 910-20R##-P0 0.010" (0.254 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 2” Wide Rectangular .2 inch wide, 10 mil thick, Red, Rectangular cross-section, Self-fus.. |