Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 32.7 kV/mm | 831 kV/in | ASTM D149 |
Westlake Plastics Tempalux® Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Dielectric Strength | 32.7 kV/mm | 831 kV/in | Arlon-SQA-TMS-020 |
Arlon 44278R018B 0.018" Uncured/Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate Design/Construction:Interleave 1: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 1: Cured Silicone RubberInterleave: LDPEUL R.. |