Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 0.339 kV/mm | 8.60 kV/in | |
Dow Corning JCR 6140 Two-part, transparent, medium modulus LED encapsulant with high transparency and medium viscosity.Information provided by Dow Corning |