Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 0.315 kV/mm @Thickness 3.17 mm |
8.00 kV/in @Thickness 0.125 in |
Unconditioned; ASTM D149 |
Garlock 9200 Nitrile Rubber Gasketing, Nylon Insert Nitrile rubber with proprietary nylon insertCombines elasticity and extensibility of rubber with strength of fabric insert. Specially compounded in varying burst strengths for almost any service co.. |