Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 30.5 kV/mm | 775 kV/in | IEC 60243-1:1998-01 |
Global EPP PA 66E Extruded Polyamide 66 Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecu.. |
|||
Dielectric Strength | 30.5 kV/mm | 775 kV/in | IEC 60250 |
Polyram PlusTek PA201 Nylon 66 for Extrusion High viscosity Nylon 66 for extrusion applications.Information provided by Polyram. |
|||
Dielectric Strength | 30.5 kV/mm @Thickness 0.400 mm |
775 kV/in @Thickness 0.0157 in |
thick |
Arkema Group Rilsan® Fine Powders Polyamide 11 Rilsan® fine powder coatings offer weatherability, long-lasting adhesion, chalk resistance, chemical resistance to aliphatic hydrocarbons, bases, salt solutions, oils, greases and other petroleum p.. |
|||
Dielectric Strength | 30.5 kV/mm | 775 kV/in | ASTM D149 |
Arlon R36338R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone Rubber Side 1, Layer 1: Uncured Silicone Rubber Substrate: Style 7628 FiberglassSide 2: Cured Silicone RubberAppearan.. |