Polymer Property : Dielectric Strength = 7700 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 303 kV/mm
7700 kV/in
Resinlab® AR 1018 Conformal Coating
Resinlab™ AR 1018 is a one-part low viscosity acrylic based conformal coating for electronic circuit boards. It possesses excellent flexibility and adhesion to many substrates. It provides excell..