Polymer Property : Dielectric Strength = 767 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 30.2 kV/mm
767 kV/in
IEC 60243-1
Lanxess Pocan® DP 1105 000000 PBT
PBT, non-reinforced, injection molding, extrusion, improved flowability
Dielectric Strength 30.2 kV/mm

@Thickness 0.400 mm
767 kV/in

@Thickness 0.0157 in
thick
Arkema Group Rilsan® Fine Powders Natural Polyamide 11
Rilsan® fine powder coatings offer weatherability, long-lasting adhesion, chalk resistance, chemical resistance to aliphatic hydrocarbons, bases, salt solutions, oils, greases and other petroleum p..