Dielectric Strength 300 kV/mm
7620 kV/in
JIS C-2318
DuPont Teijin Films Teonex® Q51 Polyester Film, 48 Gauge
Teonex® Q51 is biaxially oriented polyethylene naphthalate (PEN) film. It is slightly hazy with excellent handling properties for general purpose. It is commercially available in nominal 48 - 1000 ..