Electrical Properties Metric English Comments
Dielectric Strength 299.6 kV/mm
7609 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Melinex® SWC Polyester Film, 92 Gauge
A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi..