Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 76.26 kV/mm | 1937 kV/in | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Mylar® WC11/WC22 Polyester Film, 284 Gauge Mylar® type WC11 films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectric and good handlin.. |