Polymer Property : Dielectric Strength = 693 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 27.3 kV/mm

@Thickness 1.60 mm
693 kV/in

@Thickness 0.0630 in
in oil; ASTM D 149
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East)
XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab..
Dielectric Strength 27.3 kV/mm

@Thickness 3.20 mm
693 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS
Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a..
Dielectric Strength 27.3 kV/mm

@Thickness 3.20 mm
693 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific)
Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a..