Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 65.7 kV/mm | 1670 kV/in | |
Saint-Gobain CHR® M741 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |