Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 1.38 - 244 kV/mm | 35.0 - 6200 kV/in | Average value: 25.5 kV/mm Grade Count:249 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |